Solef® 80 000 Series Expanded PVDF is ideally suited for Oil & Gas applications such as pipe, pump or manifold insulation and many other offshore structures.Thanks to the inherent advantages of a high performance fire-retardant, chemically resistant, insulating foam - a complex pipe system, or pump housing for example can be readily and efficiently insulated and simply maintained.With a history of excellent service without failure in some of the most demanding applications, PVDF foam is suitable for many applications in this industry.
Temperature Ranking
according to the ISO 13628 part.11
Tests on PVDF and ECTFE after 1,000 hoursat high temperatures
Abrasion Resistance @ 80°C
Swelling of Solef® PVDF in Hydrocarbons
Resistance to H2S: Hydrogen Sulfide Permeability
Temperature Rating Guideline for Solef® PVDF
Creep Resistance Tests
Mechanical Properties After Immersion in Methanol
at 110°C/30 days vs 90 days(measurement made directly after immersion)
Swelling in Methanol
Swelling in Ethanol
Chemical Resistance and Temperature Ratingvs Fluorine Content
Permeability of Solef® PVDF in Alcohol
Tecnoflon® FKM Peroxide CurableTemperature Effect on P 959 in H2S 64% - EB Change
Tecnoflon® FKM Ionic CurableTemperature Effect on FOR 5381 in H2S 64% - EB Change
VPL 85540 in Norsok Fluid and Methanol(After 70hrs @ 23°C)
Norsok Fluid: Heptane/20% Cyclohexane/10% Toluene
Fuel C: Mixture 50-50% of Iso-Octane and TolueneM15: Mixture 85-15% of Fuel C and Methanol
Chemical Resistance in Hydrocarbon Blends and Methanol(336 hrs @ 60°C)
VPL 85540 vs Other Elastomers - Change in Durometer After Aging in Fluids(70 hrs @23°C)
Organic Acid Resistance10% Formic Acid, 10% Acetic Acid, 80% Dl Water(336 hrs @ 121°C)
Acid Resistance98% H2SO4(70hrs @ 150°C)
Steam Resistance(169% @ 200°C)
MaterialsFilmsAjedium Film Services